• 三腔气体
Air permeability tester
It is suitable for the detection of O2, CO2, N2 and air permeability of plastic film, composite film, high barrier material, sheet, metal foil, rubber and other materials.

Introduction


GTR-V3 Gas Transmission Rate Tester (GTR Tester) is professionally applicable to determining the gas (O2, CO2, N2) transmission rate of plastic films, composite films, high barrier materials, sheeting, metal foils, rubber, tires, and permeable membranes with differential pressure method.


Features


● High precision infrared sensor is used to ensure the testing accuracy

● Automatic humidity and temperature control to guarantee the stability of the testing environment

● All test operations are performed on a computer with testing software. User-friendly interface for easy and simplified operation.

● Test data and curves are displayed in the real time

● 3 independent test chambers for 3 test samples

● Automatic test operation by one-button clicking

● Patented pipeline flushing design ensures cleanliness of carrier gas and high testing efficiency

● Unique sample leak-proof seal installation technology enhances the seal performance of test chambers

● Meeting the requirements of USP 1207 United States Pharmacopoeia Standard for data traceability, rights management and other functions, the computerized system fully meets the needs of the pharmaceutical industry (optional)


Technical Specification


ItemParameter
ModelGTR-V3
Measurement range(film)0.1~50.000cc/㎡·24h·0.1MPa
Sample quantity3
Main sensor quantity3
Test modesingle chamber independent
Vacuum resolution0.01Pa
Vacuum degree<10Pa
Temperature control range5℃~95℃
Humidity control range0%RH,2%RH~98.5%RH±3%RH(note1)
Temperature control precision±0.05℃
Temperature resolution0.01℃
Test pressure-0.1 MPa~+0.3MPa(regular)
Air source pressure0.4 MPa~0.6 MPa
Test airO₂N₂CO₂or other gas
Interface of carrier gasФ6
Vacuum tube diameter1/4"
Calibration modeCalibration of standard film and external calibration of vacuum sensor
Sample thickness≤3mm
Sample sizeΦ97mm
Permeability area38.48 cm2
Size760 mm (L) × 575 mm (W) × 450 mm (H)
Weight88Kg
Power supplyAC100~240V   50/60Hz


Testing Principle


The pre-conditioned specimen is mounted in the gas diffusion cell to form a sealed barrier between two chambers. The lower-pressure chamber is first evacuated, followed by the evacuation of the entire cell. Gas is then introduced into the evacuated higher-pressure chamber, creating a constant pressure difference between the two chambers. The gas permeates through the specimen from the higher-pressure side to the lower-pressure side. By monitoring the pressure changes in the lower chamber, the gas permeability and other barrier properties of the specimen can be determined.


Test standard


ASTM D1434,ISO 2556,ISO 15105-1


Configuration


Standard configuration: main instrument, constant temperature controller, computer, professional software, special sampler, vacuum grease, fast quantitative filter paper, vacuum pump

Optional: sampling blade, vacuum grease, vacuum pump oil, fast quantitative filter paper, humidity generator

Note: The air source of the machine is ф 6mm polyurethane pipe. Gas source and distilled water are provided by users.

The device appearance diagram shows the standard device appearance, the appearance of customized devices may vary.