CZY-03 Adhesive Shear Adhesion Tester

›

‹

›

CZY-03 Adhesive Shear Adhesion Tester

CZY-03 Adhesive Shear Adhesion Tester is applicable for adhesives, adhesive tapes, adhesive products and relative industries. It is applicable in holding power test of pressure sensitive adhesive tapes.
Product Introduction

Introduction


CZY-03 Adhesive Shear Adhesion Tester  is applicable for adhesives, adhesive tapes, adhesive products and relative industries. It is applicable in holding power test of pressure sensitive adhesive tapes.


Features


● Stainless steel buttons, stable and durable

● 6-station supports multi-group tests

● Micro-computer controlled automatic timing, LCD screen display, accurate and reliable

● 304 stainless steel plate is used and all designs fully meet standard requirements


Technical parameters


ItemParameter
Weights1000±10g (including test plate)
Test Plate125 mm (L) × 50 mm (W) × 1.1 mm (D)
Timing Range0-99h59m59s
Number of Stations6
Instrument Dimension320(L)mm×140(B)mm×180(H)mm
Instrument Weight20kg
Standard ConfigurationMain Instrument, Test Plate, Weights, Pressing Roller


Standards


This instruments conforms to multiple international standards ASTM D3654, IS Z0237.