FCF-T01 Friction Peel Tester

›

‹

›

FCF-T01 Friction Peel Tester

FCF-T01 Friction Peel Tester can be used to test coefficient of static and dynamic friction of plastic films, sheets, foils, paper, cardboard, woven bags, fabric (fabric style test), metal-plastic composite belt for communication cable, convey belt and textile, as well as peel strength test of adhesive laminated products, medical adhesive bandage, release paper and protective films.
Product Introduction

FCF-T01 Friction Peel Tester can be used to test coefficient of static and dynamic friction of plastic films, sheets, foils, paper, cardboard, woven bags, fabric (fabric style test), metal-plastic composite belt for communication cable, convey belt and textile, as well as peel strength test of adhesive laminated products, medical adhesive bandage, release paper and protective films.


Product Features


● The instrument is professionally applicable to coefficient of friction test as well as peel strength test

● The sliding plane and the sled are treated by degaussing and remanence detection which effectively reduce the system errors

● The equipment is controlled by a microcomputer and has a 7-inch touch screen, which is convenient for users to operate and view data

● Precision differential motor drive, more smooth transmission, lower noise, more accurate positioning, better repeatability of test results

● Equipped with a micro printer and a standard RS232 interface, which facilitates external connection and data transmission between the system and the computer


Test Standards


This instruments conforms to multiple international standards ISO 8295, ISO 8510-2, ASTM D1894, ASTM D4917, ASTM D3330, TAPPI T816, TAPPI T549


Technical Specifications


ItemParameter
Measuring Range0.6kg (Customization available)
Force Resolution0.01 N
Displacement Resolution0.01 mm
Sample Thickness≤5mm (other thickness can be customized)
Sliding Plate Size63×63mm
Test ModeStripping Test, Coefficient of friction test
Display Screen7 "(65 million color TFT LCD screen)
Sled Mass200g, 500g (optional)
Bench Size120×400mm
Digital DisplayThe dynamic and static coefficient of friction are displayed
Measurement AccuracyBetter than 0.5
Sliding Speed100, 150mm/min, 1-500mm/min stepless speed (customization available)
Sliding Stroke500mm (adjustable)
Instrument Dimension900 (L)X400(W)X200mm (H)
Power SupplyAC220V±22V, 50Hz
Net Weight25kg
Environmental RequirementTemperature: 23±2℃, humidity: 50±5%RH
Standard ConfigurationMain instrument, micro printer, 200g sled, 180° stripping test fixture
Optional90° stripping test fixture, thick sample fixture, 500g non-standard sled