HST-01B Heat Seal Tester

›

‹

›

HST-01B Heat Seal Tester

HST-01B Heat Seal Tester (Laboratory Heat Sealer) is designed to determine the optimal heat seal parameters, including dwell time, sealing pressure, and sealing temperature, for plastic films, flexible composite films, plastic-coated paper, and other heat-sealable materials.
Product Introduction

HST-01B Heat Seal Tester (Laboratory Heat Sealer)  is designed to determine the optimal heat seal parameters, including dwell time, sealing pressure, and sealing temperature, for plastic films, flexible composite films, plastic-coated paper, and other heat-sealable materials.


Product Features


● Built-in microcomputer control, simple and efficient user interface

● 6 inch high-definition color LCD screen

● Digital P.I.D temperature control technology ensures that the set temperature can be reached quickly and effectively avoids temperature fluctuation

● Temperature, pressure, time and other test parameters can be directly input on the touch screen

● Patented design of sealing jaws to ensure the uniformity of heating temperature of the whole sealing surface

● The test can be started manually or by pedal switch to ensure the safety of operation personnel


Test Standards


The instrument complies multiple international standards  ASTM F2029


Technical Specifications


ItemParameter
Heat Sealing TemperatureRoom Temperature~300℃
Heat Sealing Pressure0~700Kpa
Dwell Time0.1~999.9s
Temperature Control Accuracy±0.2℃
Temperature Uniformity±1℃
Heating ModeOne-side Heating
Heat Sealing Area150 mm*10 mm
Power SupplyAC 220V 50Hz / AC 120V 60 Hz
Air Source0.7 MPa (Prepared by users)
Port SizeФ6 mm PU Tubing
Dimension547mm (L) * 200 mm (W) * 390 mm (H)
Net Weight20kg
Standard ConfigurationMain Instrument, Gas Pipeline, Power Cord➢ Optional parts: micro printer, 15# sampling knife, silicone rubber plate, high temperature solder cloth
OptionalMicro Printer, 15# Sampling Knife, Silicone Rubber Plate, High Temperature Solder Cloth