RSY-R2 Thermal Shrinkage Tester

›

‹

›

RSY-R2 Thermal Shrinkage Tester

RSY-R2 Thermal Shrinkage Tester is professionally applicable to the determination of heat shrinkage ratio of various films, heatshrinkable tubes, hard PVC films for tablets, and back-sheets in the fluid medium at different temperatures.
Product Introduction

RSY-R2 Thermal Shrinkage Tester is professionally applicable to the determination of heat shrinkage ratio of various films, heatshrinkable tubes, hard PVC films for tablets, and back-sheets in the fluid medium at different temperatures.


Product Features


● Microcomputer control, PVC menu type operation panel

● Humanized design, easy to operate

● High precision circuit processing technology, accurate and reliable test

● Liquid heating without volatile medium provides wide heating range

● Digital P.I.D temperature control monitoring technology ensures set temperature can be reached quickly and effectively avoids temperature fluctuations

● Automatic timing function to ensure test accuracy

● Standard clamp wire mesh support could make the test done smoothly

● Compact structure design, light and easy to handle

 

Test Standards


The instrument complies multiple international standards  ASTM D2732


Technical Specifications


ItemParameter
Sample Size≤140mm×140mm
Temperature RangeRoom temperature ~ 200℃
Temperature Control Accuracy± 0.3 ℃
Heating MediumOil bath
Instrument Dimension360 (L) mm x 440 (W) mm x 320 (H) mm
Weight14Kg
Operating Temperature23 ℃ + 2 ℃
Relative Humidity50% ±5%
Power SupplyAC220V50Hz