WVTR-C6 Water Vapor Transmission Rate Tester

›

‹

›

WVTR-C6 Water Vapor Transmission Rate Tester

WVTR-C6 Water Vapor Transmission Rate Tester is designed and manufactured based on the gravimetric method and can be used to test the water vapor transmission rate of plastic films, composite films, sheets, and other materials used in the packaging, medical, and construction industries.
Product Introduction

WVTR-C6 Water Vapor Transmission Rate Tester is designed and manufactured based on the gravimetric method and can be used to test the water vapor transmission rate of plastic films, composite films, sheets, and other materials used in the packaging, medical, and construction industries.


Features

 

● Based on the gravimetric method, testing of thin film sample water vapor transmission rate (WVTR) as low as 0.1g/m2•24h

● High resolution weighing sensor provides excellent system sensitivity, ensuring high accuracy.

● Wide range, high precision, automatic temperature and humidity control, easy to achieve non-standard testing

● Standard purging speed ensures constant humidity difference between inside and outside the cup

● Zero clearing before weighing to ensure the accuracy of each weighing

● Cylinder lifting mechanical structure design and intermittent weighing measurement method effectively reduces the system error

● Rapid access to temperature and humidity verification socket for users to carry out rapid calibration.

● The precise mechanical design ensures the ultra-high precision as well as high detection efficiency

● 6 permeable cups can be independently tested, the test process does not interfere with each other, and the test results are independent display.

● Large size touch screen friendly man-machine function, convenient for user operation and quick learning.

● Support test data multi-format storage, convenient data import and export.

● Support convenient historical data query, comparison, analysis and printing and other functions.


Technical Specification parameters


IndexParameter
Measuring Range 0.1~10,000g/㎡·24h(Conventional) 
 Sample Quantity 3 (independent test data) 
Measuring precision 0.01 g/m2·24h 
Testing Resolution 0.0001 g
Temperature Control Range15℃~55℃ (standard) 5℃-95℃ (Optional)
Temperature Accuracy ±0.1℃ (standard) 
Humidity Control Range 90%RH~70%RH (Standard 90%RH) 
Humidity Accuracy ±1%RH 
Purge Speed 0.5~2.5 m/s (Customization available) 
Sample Thickness ≤3 mm (Customization available) 
Measuring Area 33 cm2 
Sample Size Φ74 mm 
Testing ModeCup Method (standard), Desiccant method (optional)
Air Source Pressure0.6 MPa 
Port Size Φ6 mm PU tube
Power Supply 220VAC 50Hz / 120VAC 60Hz 
Instrument Dimension 660 mm (L) × 480 mm (W) × 525 mm (H) 
Net Weight 70Kg 


Test Principle


Using the moisture permeable cup weighing test principle, at a certain temperature, the two sides of the sample formed a specific humidity difference, the water vapor through the moisture permeable cup into the dry side of the sample, by measuring the weight of the moisture permeable cup changes with time, the water vapor permeability of the sample and other parameters.


Test Standard


ASTM E96, ASTM D1653, TAPPI T464, ISO 2528, JIS Z0208


Configuration


Standard Configuration: Instrument, Computer, Testing Software, Communication Cable, Sample Cutter, Vacuum Seal Grease, Printer

Optional: Package/Container Test Accessories and Temperature Control Device

Note: Air source and distilled water (Prepared by the user)

Note: The manufacturer reserves the rights to modify the configurations of the instrument.

Related Product Recommendations

Send Us Your Inquiry

SUBMIT

*We respect your privacy and are committed to protecting it through our compliance with our Privacy Policy.