FBT-01 Falling Ball Impact Tester

›

‹

›

FBT-01 Falling Ball Impact Tester

The falling ball impact tester is suitable for testing the instantaneous impact of plastic, plexiglass, building materials, ceramics, coatings and other test samples to test the damage degree of materials.
Product Introduction

Product Details


The falling ball impact tester is suitable for testing the instantaneous impact of plastic, plexiglass, building materials, ceramics, coatings and other test samples to test the damage degree of materials.


Parameters


● Steel ball weight: 112g, 198g, 225g, 357g, 533g

● Drop height: 20~2000mm

● Resolution: 0.1

● Drop height scale: minimum indication 1cm

● Machine size: W400 x D450 x H2200mm

● Machine weight: 50kg

● Power source: 1 #, 220V, 5A or specified