GPT-01 Automatic glass bottle internal pressure tester

›

‹

›

GPT-01 Automatic glass bottle internal pressure tester

GPT-01 automatic glass bottle internal pressure tester is designed and produced according to ASTM C147-76 (reviewed in 81) method B (linear pressurization method) of the American Society for Materials
Product Introduction

GPT-01 automatic glass bottle internal pressure tester is designed and produced according to ASTM C147-76 (reviewed in 81) method B (linear pressurization method) of the American Society for Materials, in line with GB/T 4546-2008 "Glass container internal pressure test method". National standard YBB00172003-2015 "internal pressure test method" and ISO/CD7458 "Glass container internal pressure test method" international standards. It is mainly used for the internal pressure test of glass beer bottles, soda bottles, cola bottles and glass infusion bottles Check.


Features

 

1. High test accuracy, large range, the maximum test pressure is 6.00Mpa.

2. High test speed, the pressure increasing time for each test bottle is not more than 10 seconds, and for ordinary tests it is about 4 seconds (the end point, the pressure is 1.60Mpa).

3. High degree of automation, easy to use, automatic fault detection and common fault prompts and equipped with a printer.

4. High reliability. Advantages of foreign products, key materials, components using imported parts.

5. This tester is suitable for glass bottle factory, beer brewery, beverage factory and relevant quality inspection department to batch glass bottles.


Technical Specification parameters


Measuring pressure range

0.50 ~ 6.0Mp

Number of workstations2
Pressure resolutions0.01MPa
Pressure test errorless than 1.5% F.S
Test bottles per minuteabout 5 ~ 10 pieces
Boost rate errorsless than 5%
bottle clamp diameter

24 ~ 29mm (other specifications need to be customized

Ambient temperature ranges0 to 40 ° C
Ambient humidity ranges

less than 95% relative humidit

Power supply voltage range

220 VAC ± 5% (grounding must be good)

User provided

10 Air pressure 0-0.8mpa User provided

 (pressure boost rate can meet 0.4MPa/s± 0.1MPa /s, 0.58MPa/s± 0.1MPa /s, 1.0MPa/s±0.2MPa/s)